Enhancement of copper dissolution by mechanochemical activation of ...
After sieving, 30 g of samples were grinded for 1 h, either by a planetary ball mill (High G, Kurimoto ltd., JAPAN), or by a vertical stirred ball mill (Powder Lab, Nippon Coke Engineering Co., Ltd, JAPAN), both equipped with 10 mm zirconia balls as grinding media. In the planetary ball mill, rotation to revolution speed ratio was set at 0. ...